Dear Sirs,
Please give me information regarding welding (Resistance Butt Welding)
1. Current Required ? as per Diameter & Carbon % of steel wire
2. Annealing Time
Please give me information regarding welding (Resistance Butt Welding)
1. Current Required ? as per Diameter & Carbon % of steel wire
2. Annealing Time
Please Log in to join the conversation.
- Archived Forum Admin
- Topic Author
- Offline
- Platnium Boarder
12 years 10 months ago #1143 by Archived Forum Admin
Replied by Archived Forum Admin on topic Re: Welding Parameters.....
Hallo RBWL:
I think it is a good idea for you to contact this organization and ask for information about training
www.slv-duisburg.de/home_slv_duisburg_e.0.html
As my lecturer in university ones upon said:
"the result of a welding procedure depends of the character of the welder"
so it it very important to control the process and to inspect the result.
Best regards
Juan Carlos González Villar
Kabel.Consult.Ing
www.kabelconsulting.de
This email address is being protected from spambots. You need JavaScript enabled to view it.
I think it is a good idea for you to contact this organization and ask for information about training
www.slv-duisburg.de/home_slv_duisburg_e.0.html
As my lecturer in university ones upon said:
"the result of a welding procedure depends of the character of the welder"
so it it very important to control the process and to inspect the result.
Best regards
Juan Carlos González Villar
Kabel.Consult.Ing
www.kabelconsulting.de
This email address is being protected from spambots. You need JavaScript enabled to view it.
Please Log in to join the conversation.
- Archived Forum Admin
- Topic Author
- Offline
- Platnium Boarder
12 years 10 months ago #1144 by Archived Forum Admin
Replied by Archived Forum Admin on topic Re: Welding Parameters.....
1.Current Required ? as per Diameter & Carbon % of steel wire
The current required to make a weld on steel is dependent upon the size of rod being welded, for example .062” diameter will require 10 amps. at 115 volts, while .750” diameter would require 50 amps. at 460 volts. Carbon content does not determine the amount of current for welding however the higher the carbon content the more there is a need to anneal. 1008 material for example requires Little or no annealing depending on the application while 1050 would definitely need to be annealed.
2.Annealing Time
There are many variables regarding annealing; size of rod, welder settings and temperature needed to anneal that particular carbon content.
I hope this helps if not please try to be more specific with the questions.
The current required to make a weld on steel is dependent upon the size of rod being welded, for example .062” diameter will require 10 amps. at 115 volts, while .750” diameter would require 50 amps. at 460 volts. Carbon content does not determine the amount of current for welding however the higher the carbon content the more there is a need to anneal. 1008 material for example requires Little or no annealing depending on the application while 1050 would definitely need to be annealed.
2.Annealing Time
There are many variables regarding annealing; size of rod, welder settings and temperature needed to anneal that particular carbon content.
I hope this helps if not please try to be more specific with the questions.
Please Log in to join the conversation.
- Archived Forum Admin
- Topic Author
- Offline
- Platnium Boarder
12 years 10 months ago #1145 by Archived Forum Admin
Replied by Archived Forum Admin on topic Re: Welding Parameters.....
Thank you sir for giving usefull information