Die Galling

Adhesion buildup of metal onto the surface of the die caused by the breakdown of the lubricant film on the wire surface, resulting in metal-to-metal contact. This results in excessive friction, higher die temperatures and a rough surface in the die that results in scratches on the drawn wire.